Two reports, one failure mode
On 2 November 2026 the Chongqing Emergency Management Bureau published the investigation report on the 12 April 2026 burst of the penstock at the Qingyandong fourth-stage hydropower station, run by Chongqing Xingfu Power Development. The report names four causes. The plant did not implement a safety risk grading control system. It did not eliminate the safety hazard of corrosion thinning of the pressure steel pipe wall. It did not carry out welding work on the pressure steel pipe in accordance with the specification. And it did not define safety management measures for the crossing of power generation operation with anti-corrosion reinforcement work. Four people died and the direct economic loss was about 6.99 million yuan.
Ten days earlier, on 8 October 2026, a connecting line in the 1 million tonne per year diesel hydrotreating unit of Ningxia Baoruolong Petrochemical ruptured between the high-pressure and high-low-pressure heat exchangers. The Ministry of Emergency Management subsequently published the accident case documentation and, on 22 October, issued a notice requiring video-based warning training on hydrotreating accidents across the country. The line was nominally 300 mm diameter, A106 Grade B, with a 21.4 mm nominal wall, running at 230 °C and 9.7 MPa gauge, designed for 250 °C and 10.19 MPa gauge, and installed at about 5.8 m height.
The published case documentation gives the wall thickness measurements directly. The design thickness was 21.4 mm. At the thinnest point, measured on the outer bend of the third elbow above the high-pressure exchanger outlet, the wall had thinned to about 3 mm. The report identifies three corrosion mechanisms working together. The feedstock was coal tar, with high impurities and a deteriorating quality; nitrogen was early hundreds of ppm and later 1100 to 1200 ppm, and chloride had been at 2 to 3 ppm for a long period with no defined control threshold. Water injection, the key corrosion control point in a hydrotreating unit, was left at the original fixed design rate and never recalculated as the feed deteriorated, and neither injection branch had a flow meter. And the line had been run above its design temperature: from 14 September 2026 the DCS trend shows pipe temperature rising from around 240 °C to 258 °C, above the 250 °C design maximum.
The investigation also found the inspection gap. Every periodic inspection since 2020 failed to reach the rupture location at 5.8 m height. Only the low-lying elbows that were easy to access were spot-checked, and routine fixed-point thickness measurement had the same problem.
What the reports say, and what they do not
It is worth being precise about what these two documents are. They are official investigation reports, published by the responsible government authority, and they set out causes, deficiencies and recommended enforcement. They are not failure analyses of a specific alloy, and they do not name a material grade as the root cause. The Baoruolong line was A106 Grade B carbon steel, verified from the published parameter table. The report does not argue that carbon steel was the wrong choice for the duty. It argues that the wall that was installed thinned in service, that nobody measured the high-lying points where it thinned, that the process was running above its design temperature, and that the corrosion control parameters were not managed against a changing feed.
That distinction matters to anyone buying alloy pipe rather than carbon steel pipe. A material specification governs the wall thickness that arrives at your site, the chemistry, the mechanical properties and the marking. It does not govern what happens to that wall in the fifth year of service. The reports describe the second thing: a wall that met its specification on the day of delivery, thinned unmeasured where inspection never reached.
The clauses a buyer can actually invoke
The material specifications for steel pipe and forgings are, in the main, silent on corrosion allowance. A search of the entire local ASME BPVC Section II text cache returns the phrase “corrosion allowance” in only three specifications — SA-263, SA-264 and SA-265, the clad plate specifications, where it appears in the context of cladding supplied for corrosion allowance purposes. It appears zero times in SA-106, SA-312, SA-790, SA-789, SA-999, SA-961, SA-182, SA-403, SB-829, SB-775 and SB-861. Corrosion allowance is a design code parameter. What the material volume does give you are the clauses that decide how the delivered wall is verified and what the mill must state about it.
SA-106 clause 13.1 requires that except as allowed by 13.2, 13.3 and 13.4, each length of pipe shall be subjected to the hydrostatic test without leakage through the pipe wall. Clause 13.2 allows the full body of each pipe to be tested with a nondestructive electric test described in Section 14, at the option of the manufacturer or where specified in the purchase order. Clause 13.3 is the one most buyers miss: where specified in the purchase order, pipe may be furnished without the hydrostatic test and without the nondestructive electric test, and in that case each length so furnished shall include the mandatory marking of the letters NH. A pipe order that does not address 13.3 leaves the decision open.
Clause 12.1 makes the point from the other end of the certificate. Although testing is not required, pipe shall be capable of meeting the flattening test requirements of Supplementary Requirement S3, if tested. The capability is guaranteed; the test is not performed unless you invoke it.
| Order point | Clause | What the specification says |
|---|---|---|
| Hydrostatic test on every length | SA-106 §13.1 | Each length tested without leakage through the pipe wall, except as allowed by 13.2, 13.3, 13.4 |
| Electric test as an alternative | SA-106 §13.2 | Full body of each pipe may be tested by a nondestructive electric test, at the manufacturer’s option or where specified in the purchase order |
| Supply without either test | SA-106 §13.3 | Permitted where specified in the purchase order; each such length must carry the marking NH |
| Flattening test | SA-106 §12.1 | Pipe shall be capable of meeting S3, if tested — capability is guaranteed, the test is not automatic |
| Pipe ordered for bending and flanging | SA-106 §1.1 | Pipe shall be suitable for bending, flanging and similar forming operations, and for welding |
SA-106 clause 1.1 is worth a second look. Pipe ordered under this specification shall be suitable for bending, flanging, and similar forming operations, and for welding. When the steel is to be welded, it is presupposed that a welding procedure suitable to the grade of steel and intended use or service will be utilized. The Chongqing report names as one of its four causes that the pressure steel pipe was not welded in accordance with the specification. SA-106 presupposes a suitable procedure; the report found the work was not done to specification.
SA-106 Table 1 shows Grade B carbon as C 0.30 max with footnote B, manganese 0.29 to 1.06, phosphorus and sulfur 0.035 max, silicon 0.10 min, and chromium, copper, molybdenum, nickel and vanadium each at 0.40 max with a combined 1 per cent limit. Grade B is a carbon steel with a composition designed for weldability and toughness, not for a corrosive process stream.
Where the purchase order carries the weight
Two questions a buyer can put into a specification.
First, how is the delivered wall thickness going to be verified beyond the mill test report. SA-999 clause 25.2 requires a test report including the heat number, heat analysis, product analysis if specified or required, tensile properties and the results of the other required tests, and clause 25.1 requires a certificate of compliance stating that the product was manufactured, sampled, tested and inspected in accordance with the specification. A signature or notarization is not required, however the document shall be dated.
Second, what is the inspection and thickness-measurement regime going to be, and does it reach the geometry the Baoruolong report describes. The reports make a reproducible point: an inspection regime that only reaches accessible low-lying components will miss a failure at 5.8 m, and a fixed-point thickness measurement plan with the same reach problem will miss it too. That is a scoping question for the inspection and test plan, not a materials question, and it is the one question a buyer can answer before the pipe is installed.
What these reports cannot tell you is which alloy to specify, or what corrosion rate to design for. Section II carries no corrosion rates, no concentration limits and no service-life predictions. What they do establish is that a wall of verified thickness, inspected at a reach that matches the geometry, is the last line of defence — and that the specification controlling that wall is the purchase order.
Send us the alloy grade, the specification, the size range and the service conditions for your next enquiry and we will return a written material proposal against the ASME specification that governs the product form you need. Message our export desk on WhatsApp or use the our export enquiry form to get a quotation request started.
Related products: nickel alloy seamless pipe and tube · Inconel 625 seamless pipe · Hastelloy C-276 seamless pipe · pipe and tube. Supplied to the applicable ASTM / ASME specifications with EN 10204 3.1 mill test certificates; confirm grade, size and quantity with our engineers.